Basic Info | Layer Height(mm) | 0.05 |
---|---|---|
Retract Speed(mm/min) | 150 | |
Bottom Layers | Layer Count | 6 |
Exposure Time(s) | 25-35 | |
Lifting Distance(mm) | 6 | |
Lifting Speed(mm/min) | 60 | |
Light-off Delay(s) | 10 | |
Transition Layers | Layer Count | 6 |
Normal Layers | Exposure Time(s) | 2.0-2.5 |
Lifting Distance(mm) | 6 | |
Lifting Speed(mm/min) | 60 | |
Light-off Delay(s) | 10 |
Basic Info | Layer Height(mm) | 0.05 |
---|---|---|
Retract Speed(mm/min) | 150 | |
Delay(ms) | 6 | |
Burn Layers | Layers(Numbers) | 25-35 |
Cure Time(ms) | 6 | |
Lift Height(mm) | 60 | |
Up Speed(mm/min) | 10 | |
Normal Layers | Cure Time(ms) | 6 |
Lift Height(mm) | 2.0-2.5 | |
Up Speed(mm/min) | 6 |
Basic Info | Layer Height(mm) | 0.05 |
---|---|---|
Retract Speed(mm/min) | 150 | |
Bottom Layers | Layer Count | 6 |
Exposure Time(s) | 25-35 | |
Lifting Distance(mm) | 6 | |
Lifting Speed(mm/min) | 60 | |
Light-off Delay(s) | 10 | |
Normal Layers | Exposure Time(s) | 2.0-2.5 |
Lifting Distance(mm) | 6 | |
Lifting Speed(mm/min) | 60 | |
Light-off Delay(s) | 10 |
Basic Info | Layer Height(mm) | 0.05 |
---|---|---|
Retract Speed(mm/min) | 150 | |
Bottom Layers | Layer Count | 6 |
Exposure Time(s) | 25-35 | |
Lifting Distance(mm) | 6 | |
Lifting Speed(mm/min) | 60 | |
Transition Layers | Layer Count | 6 |
Normal Layers | Exposure Time(s) | 2.0-2.5 |
Lifting Distance(mm) | 6 | |
Lifting Speed(mm/min) | 60 | |
Waiting Mode   During Printing | Mode | Resting time |
Rest Time After Retract(s) | 3 |
1. These resin parameters have been determined with a temperature of 25°C and relative humidity of 75%. A test print was performed in a well-ventilated indoor space.
2. We used the Phrozen_XP_finder.stl (Download here) test print file to determine these resin parameters. Please use this STL file to test out the resin parameters before you begin printing. To learn more about how to dial in any resin with an XP_finder.
3. Phrozen Sonic Mighty 8K can only read CTB files by Chitubox or Lychee. You may also use any other slicing software if you prefer to do so.
4. If your prints fail to stick onto the building plate, try increasing the bottom layer exposure time or check out our Help Center.